Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 30.0 - 345 g
30.0 - 345 g
Average value: 131 g Grade Count:56
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Elmendorf Tear Strength TD 30.0 - 920 g
30.0 - 920 g
Average value: 660 g Grade Count:27
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..