Polymer Property : Elmendorf Tear Strength TD = 264 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 264 g
264 g
ASTM D1922
NOVA Chemicals Novapol® LF-0225-B LDPE Clarity Film Resin  (discontinued **)
Features: High optical clarityExcellent processability Applications: Produce and bakery filmLinersTextile packaging filmGeneral packaging requiring high clarity filmInformation provided by Nova Chem..