Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 26.4 g | 26.4 g | ASTM D1922 |
LG Chemical SEETEC SF318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |
|||
Elmendorf Tear Strength TD | 26.4 g | 26.4 g | ASTM D1922 |
LG Chemical SEETEC SN318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |