Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 245 g | 245 g | ASTM-D1922 |
Braskem TN2020 EVA General Film Copolymer TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures.. |