Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 230 g
230 g
Kraton® D1102 + HDPE blend (20/80)
Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..
Elmendorf Tear Strength TD 230 g
230 g
ISO 6383-2
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and..
Elmendorf Tear Strength TD 230 g
230 g
ASTM D1922
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl..