Polymer Property : Elmendorf Tear Strength TD = 1800 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 10.0 - 1800 g
10.0 - 1800 g
Average value: 279 g Grade Count:65
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..