Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 178 g | 178 g | ASTM D1922 |
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low.. |