Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 422 - 1350 g | 422 - 1350 g | Average value: 620 g Grade Count:18 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |