Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 1033 g
1033 g
ASTM D1922
Dow ELITE™ 5100G Enhanced Polyethylene Resin
™ 5100G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers excellent impact strength, good tensile and puncture properties for thick and thin gauge industrial and consume..