Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 101000 g | 101000 g | ASTM D1922 |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |