Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Transverse Strength | >= 70.0 MPa | >= 10200 psi | 2nd Grade, at max sample load |
Kazanorgsintez PC-007 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Transverse Strength | >= 70.0 MPa | >= 10200 psi | at max sample load |
Kazanorgsintez PC-010 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of die-casting.Information Provided by Kazanorgsintez |