Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 993 MPa | 144000 psi | Typical, Transverse Direction |
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections Description: CLC 1.2738 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, Nickel carbon and manganese additions are optimized to have a fully .. |
|||
Tensile Strength, Ultimate | 993 MPa | 144000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 30% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Ultimate | 993 MPa | 144000 psi | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |