Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 682 MPa | 98900 psi | Typical Annealed |
ATI Allegheny Ludlum Moly Permalloy Electrical Alloy An alloy with exceptionally high magnetic permeability, very low coercive force, very low core losses, and low reminance by magnetic field annealing. The alloy finds application in magnetic shieldi.. |