Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 669 - 772 MPa | 97000 - 112000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 669 MPa | 97000 psi | |
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Tensile Strength, Ultimate | 669 MPa @Temperature 70.0 °C |
97000 psi @Temperature 158 °F |
transverse |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-8 (UNS S20153) AL 201LN™ is a special composition of Type 201 specifically for sub-zero temperature service as welded tanks and vessels. This alloy has replaced the familiar 300 series stainless such as type 301.. |