Tensile Strength, Ultimate 96.1 MPa
13900 psi
Shinil Chemical SHINCON PC Electro Conductive Polymer
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's ..
Tensile Strength, Ultimate 96.1 MPa
13900 psi
Shinil Chemical SHINCON PSU-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Tensile Strength, Ultimate 96.1 MPa
13900 psi
ISO 527-1, 2
Polyplastics Duranex® 304SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Tensile Strength, Ultimate 96.1 MPa
13900 psi
DIN 53455; ASTM D638
Kolon SPESIN® KP213G15 Flame Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..