Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 652 MPa @Temperature 649 °C |
94600 psi @Temperature 1200 °F |
|
Kennametal Stellite Deloro® 208 PM cast Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s.. |