Polymer Property : Tensile Strength, Ultimate = 940 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 6.48 MPa
940 psi
Dow Corning SILASTIC® T-4 RTV SILICONE RUBBER BASE & T-4 O CURING AGENT
Translucent, oil bleeding high strength silicone mold making rubber that features high tear with fast cure. Suited for prototype design and production tooling. Silastic T-4 O is recommended for use ..
Tensile Strength, Ultimate 6.48 MPa
940 psi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 2250 UT Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 6.48 MPa
940 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Tensile Strength, Ultimate 6.48 MPa
940 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..