Tensile Strength, Ultimate 63.7 MPa
9240 psi
ASTM D1708
Daelim H&L Plavis-C DF Conductive Polyimide Bearing
Direct Formed. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grades:PL..
Tensile Strength, Ultimate 63.7 MPa
9240 psi
ASTM D1708
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca..
Tensile Strength, Ultimate 63.7 MPa
9240 psi
ASTM D1708
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing
Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the ..
Tensile Strength, Ultimate 63.7 MPa
9240 psi
ASTM D1708
Daelim H&L Plavis-ESD DF Polyimide Bearing
Direct Formed. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis info..