Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 920 - 1100 MPa | 133000 - 160000 psi | Sintered Only |
MarkeTech 95-3-2 Tungsten Alloy, AMS-T-21014 Class 3 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Ultimate | 920 - 1100 MPa | 133000 - 160000 psi | Sintered Only |
MarkeTech 96-3-1 Tungsten Alloy, AMS-T-21014 Class 3 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Ultimate | 920 - 1100 MPa | 133000 - 160000 psi | Sintered Only |
MarkeTech 97-2-1 Tungsten Alloy, AMS-T-21014 Class 4 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Ultimate | 920 MPa | 133000 psi | |
Haynes 556® alloy, 40% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |