Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 627 MPa @Temperature 538 °C |
90900 psi @Temperature 1000 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 627 MPa | 90900 psi | |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Ultimate | 627 MPa | 90900 psi | |
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |