Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.963 MPa | 1445 psi | cured 8 hours @ 93°C |
Abatron AboCast 8110-8/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |