Polymer Property : Tensile Strength, Ultimate = 882.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Crucible Steel 21-2N Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Crucible Steel 21-4N (JIS SUH35) Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Crucible Steel 21-4NNb Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Crucible Steel 23-8N Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Crucible Steel 422 (JIS SUH616) Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Crucible Steel SUE52 Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Crucible Steel 214NS (JIS SUH36) Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Crucible Steel SIL 10N Martensitic Steel
Information provided by Crucible Specialty Metals.