Polymer Property : Tensile Strength, Ultimate = 862 MPa
Polymer Property :
Tensile Strength, Ultimate =
862 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
758
-
862
MPa
110000
-
125000
psi
Eagle Brass 70265 XP175, Hard
Information provided by Eagle Brass Company