Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.590 MPa | 85.6 psi | ASTM D 638 |
REXtac Rextac® RT 2732 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good tack, and very long open timeApplications: Component of hot mel.. |