Polymer Property : Tensile Strength, Ultimate = 844 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.82 MPa
844 psi
Colorite Polymers Flexchem 3551-02 Vinyl Compound
Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut..