Polymer Property : Tensile Strength, Ultimate = 841 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.80 MPa
841 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Trefsin® 3201-65 W305 Thermoplastic Rubber  (discontinued **)
A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t..
Tensile Strength, Ultimate 5.80 MPa
841 psi
ASTM D638
Multibase Multi-Flex® TPE A 5904 LC BLK
Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and fe..
Tensile Strength, Ultimate 5.80 MPa
841 psi
Dow Corning SE 4400 KIT
Two-part, grey, heat cure, flowable, thermally conductive, UL V-0.Information provided by Dow Corning
Tensile Strength, Ultimate 5.80 MPa
841 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Trefsin® 3101-65 W305 Thermoplastic Rubber  (discontinued **)
A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec..