Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 834 MPa

@Temperature 600 °C
121000 psi

@Temperature 1110 °F
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy
Applications include diesel engine valves, and injection mold screws.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinati..
Tensile Strength, Ultimate 834 MPa

@Thickness 3.20 mm
121000 psi

@Thickness 0.126 in
Sheet
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Ultimate >= 834 MPa
>= 121000 psi
Crucible Steel JIS SUH600 Martensitic Steel
Information provided by Crucible Specialty Metals.
Tensile Strength, Ultimate 834 MPa

@Temperature 427 °C
121000 psi

@Temperature 801 °F
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..