Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.72 MPa
830 psi
Silicone Property; ASTM D412
Arlon 54B12R006 Silicone Rubber/Fiberglass Laminate
Cured silicone rubber with a fiberglass substrate.
Tensile Strength, Ultimate 5.72 MPa
830 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3860M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer..