Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 569 MPa

@Temperature 649 °C
82500 psi

@Temperature 1200 °F
Kennametal Stellite Stellite® STAR with P/M Processing
Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa..
Tensile Strength, Ultimate 569 MPa

@Temperature 538 °C
82500 psi

@Temperature 1000 °F
Haynes HR-160® alloy, solution annealed sheet
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Ultimate 569 MPa

@Temperature 316 °C
82500 psi

@Temperature 601 °F
Carpenter Gall-Tough® Stainless
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1..
Copyright © lookpolymers.com All Rights Reserved