Tensile Strength, Ultimate 29.6 - 54.2 MPa
4290 - 7850 psi
Average value: 40.2 MPa Grade Count:6
Overview of materials for Silicone Polyurethane, Polycarbonate Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim..