Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.2 - 53.0 MPa
5690 - 7690 psi
Average value: 47.9 MPa Grade Count:13
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 33.0 - 53.0 MPa
4790 - 7690 psi
Average value: 43.6 MPa Grade Count:28
Overview of materials for PVC/Acrylic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate ..