Polymer Property : Tensile Strength, Ultimate = 769.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 769.5 MPa
111600 psi
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C)
Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 2150°F (1180°C)/5 minutes/AC. This produces ASTM grain size 5.5. Other property values are ty..