Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 53.0 MPa | 7680 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN173HI4 High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 53.0 MPa | 7680 psi | ASTM D412 |
SK Chemicals SKYTHANE® 198A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 53.0 MPa | 7680 psi | ASTM D412 |