Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 - 52.4 MPa
2900 - 7600 psi
Average value: 36.3 MPa Grade Count:88
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..