Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5205 MPa | 754900 psi | |
Carpenter Micro-Melt® 10 Tough Treated Tool Steel (AISI A11) Micro-Melt® 10 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with go.. |