Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 731 MPa

@Temperature -73.0 °C
106000 psi

@Temperature -99.4 °F
Transverse
Carpenter 20Cb-3® Stainless Steel
Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re..
Tensile Strength, Ultimate 731 MPa

@Temperature 427 °C
106000 psi

@Temperature 801 °F
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Ultimate 731 MPa
106000 psi
Haynes Hastelloy® C-22® alloy, GMAW, as welded, unnotched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..