Polymer Property : Tensile Strength, Ultimate = 7210 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 49.7 MPa
7210 psi
ASTM D638
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag..