Polymer Property : Tensile Strength, Ultimate = 7100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 49.0 MPa
7100 psi
ASTM D638
Nylene® Vexel™ B12U FR Un-reinforced, Flame Retardant PBT
Description: Vexel™ B12U FR is an un-reinforced, flame retardant PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources ..
Tensile Strength, Ultimate 49.0 MPa
7100 psi
ASTM D412
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane
Type: Estane® ALR PC95A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi..