Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.186 MPa | 1042 psi | ARM 201 fluid immersion, 70 hrs. at 275°F; ASTM D1414 |
Freudenberg Simrit N456 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |