Polymer Property : Tensile Strength, Ultimate = 69000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 421 - 476 MPa
61000 - 69000 psi
Eagle Brass 210 Gilding Metal, Extra Spring
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
Tensile Strength, Ultimate 393 - 476 MPa
57000 - 69000 psi
Eagle Brass 425 Tin Brass 2%, 1/2 Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Ultimate 386 - 476 MPa
56000 - 69000 psi
Eagle Brass 735 Nickel Silver 18%, 1/4 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company