Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.6 MPa
9960 psi
DIN 53455; ASTM D638
Kolon SPESIN® KP513FLBL Multi Reinforced PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Tensile Strength, Ultimate 68.6 MPa
9960 psi
ASTM D638
Kolon Kocetal® CL704 Reinforced Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Tensile Strength, Ultimate 68.6 MPa
9950 psi
ASTM D3574E
Mearthane Durethaneâ„¢ M DM-640A Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
Tensile Strength, Ultimate 68.6 MPa
9960 psi
Shinil Chemical SHINSTAT PC Electrostatic Control Polymer Injection Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Tensile Strength, Ultimate 68.6 MPa
9960 psi
ASTM D638
SK Chemicals SKYTHANE® U0351C Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 68.6 MPa
9960 psi
ASTM D638
SK Chemicals SKYTHANE® UB220 Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Tensile Strength, Ultimate 68.6 MPa
9950 psi
ASTM D1708
Daelim H&L Plavis-ESD CM Polyimide Bearing
Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis..