Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 625 - 675 MPa | 90600 - 97900 psi | T direction |
ArcelorMittal Speed 35-510 Electrical Steel Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |