Polymer Property : Tensile Strength, Ultimate = 659 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 659 MPa
95600 psi
statistical analysis gives AVG -3STD at 620 MPa
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate
Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part..