Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 657 MPa
95300 psi
30% Cold Worked
AK Steel 409 ULTRA FORM® Stainless Steel
AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and ..