Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 645 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 645 MPa

@Temperature 540 °C
93500 psi

@Temperature 1000 °F
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Copyright © lookpolymers.com All Rights Reserved