Tensile Strength, Ultimate 441.2 - 490 MPa
63990 - 71100 psi
International Mold Steel Porcerax II Sintered, Porous Mold Steel
Description: Porcerax II is a sintered, porous metal with porosity in the range of 20 to 30% by volume. A system of interconnected pores with an average diameter of 7 or 20 micron is dispersed throu..