Polymer Property : Tensile Strength, Ultimate = 634 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4.37 - 63.2 MPa
634 - 9170 psi
Average value: 46.7 MPa Grade Count:15
Overview of materials for Polycarbonate-Urethane
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr..