Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.96475 - 43.5749 MPa @Temperature -40.0 - 85.0 °C |
430.001 - 6320.01 psi @Temperature -40.0 - 185 °F |
Average value: 23.0 MPa Grade Count:1 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |