Polymer Property : Tensile Strength, Ultimate = 63.16 MPa
Polymer Property :
Tensile Strength, Ultimate =
63.16 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
63.16
MPa
9161
psi
Phenolic 35%, Carbon fabric 65%
Phenolic - Monsanto "SC 1008". Carbon fabric - "VCA"