Polymer Property : Tensile Strength, Ultimate = 626 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 626 MPa

@Temperature 760 °C
90800 psi

@Temperature 1400 °F
Kennametal Stellite Deloro® 208 PM cast
Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s..